pe-based handstyle

PE-based Bag-Film

  • Maximizing recyclability for international sales markets
  • Barriers made of: EVOH < 5%, MBP (Medium Barrier Polymer), SiOx, metallized
  • Equipment variants: firm sealing, easy peel, laser perforation, metallized, anti-fog, resealable (zipper)
  • PE sealing medium with extremely low melting point for the best possible packaging performance
  • Suitable for HFFS, VFFS and stand-up pouches with good processability on conventional packaging systems

85 – 135 °C sealing temperature

> 90% recyclability

Recyclability (%)

Thickness

(µm)

Oxygen barrier

(cm3 / m3 / Bar / day)

Water vapour barrier

(g / m3 / Bar / day)

sealing temperature

(°C)

HFFS

Flowpack

(TPM)

VFFS

(TPM)

HFFS

SBB

(TPM)

> 90

> 60

< 2, (Medium Barrier ca. 30)

< 1

85 - 135

ca. 60

ca. 55

ca. 45

The PE-based bag film has an initial sealing point (SIP) of 85°C. This means that the seal seam strength is already given at low temperatures. This shifts the entire process temperature window by 25°C compared to conventional mixed laminates. This means that the recyclable solution achieves good packaging performance.

PE-based Top-Film

  • Maximizing recyclability for international sales markets
  • Barriers made of: EVOH < 5%, PVOH, SiOx, metallized
  • Equipment variants: firm sealing, easy peel, antifog
  • For sealing PE thermoforming films

85 – 135 °C sealing temperature

> 90 % recyclability

Recyclability

(%)

Thickness

(µm)

Oxygen barrier

(cm3 / m3 / Bar / day)

Water vapour barrier

(g / m3 / Bar / day)

sealing temperature

(°C)

> 90

> 60

< 2

< 1

85 - 135